The effect of Hot Isostatic Pressing on the MT sample densities
(Belgrade : Serbian Ceramic Society, 2015)
Mechanically activated powders (0, 10, 40, 80 and 160 minutes) were formed by isostatic pressure 300 MPa to cylindrical green bodies (φ 12 mm). First set of samples was sintered at 1300°C for 30 min in air (heating rate ...
VII International Conference on Mechanochemistry and Mechanical Alloying INCOME 2011: Programme and the Book of Abstracts
(Belgrade : Materials Research Society of Serbia, 2011)
The INCOME series of conferences initiated by International Mechanochemistry Association [an associate member of International Union of Pure and Applied Chemists (IUPAC)] has served as a common platform to bring together ...
Sintering of Zinc-Titanate
(Atlantis Press, 2016)
Sintering kinetics of the mechanically activated ZnO-TiO2 system was studied. Mixtures of ZnO and TiO2 powders were mechanically activated using a high-energy ball mill for different time intervals from 0 to 300 min. Formal ...
Surface characterisation of mechanochemicaly activated carbon cloth
(Belgrade : Materials Research Society of Serbia, 2013)
Adsorption on activated carbon cloth is an efficient procedure for removing pollutants from wastewaters, because this material possesses large specific area and high adsorption capacity. In
this study the activated carbon ...
The Morphological Characterization of Mechanically Activated ZnO Powder
(Belgrade : Serbian Ceramic Society, 2014)
The authors investigated the morphological characteristics of mechanically activated ZnO powder. ZnO powder was mechanically activated for 2, 5, 10 and 30 minutes in a planetary ball mill. Mechanical activation introduces ...
Influence of synthesis parameters and thermal treatment on functional properties of Fe3O4-BaTiO3 multiferroics obtained by mechanical activation
(Belgrade : Serbian Ceramic Society, 2017)
Mechanical activation of a mixture of polycrystalline powders Fe3O4 (50% wt.) and BaTiO3 (50% wt.) was performed in a planetary ball-mill, with different milling times (3 h, 6 h and 12 h). Average crystallite size determined ...
Influence of mechanical activation on MgO-TiO2 system
(Belgrade : Institute of Technical Sciences of SASA, 2008)
In this paper the influence of mechanical activation on MgO-TiO2 system has been investigated. Mixtures of MgO-TiO2 were mechanically activated using high-energy planetary ball mill during 0, 5, 10, 20, 40, 80 and 120 ...
Kinetics of Mechanically Activated TiO2-based Oxides Followed by DTA
(Belgrade : Serbian Ceramic Society, 2012)
TiO2-based materials are widely used in production of ceramic capacitors and semiconductors. The conventional method of ceramics synthesis relies on the solid-state reaction between TiO2 and other compounds (BaCO3, BaO, ...
Synthesis of LiFePO4 by mechanical stressing and thermal annealing
(Belgrade : Materials Research Society of Serbia, 2014)
Mechanical activation can be regarded as a multi-step process with changes in the energetic parameters and the amount of accumulated energy of solids in each step. Here we report the influence of mechanochemical processing ...
Structural characterization of mechanically activated MgO-TiO2 system
(Belgrade : Materials Research Society of Serbia, 2011)
Mixtures of MgO-TiO2 powders were mechanically activated in a planetary ball mill for time interval from 0 to 120 minutes. On thus obtained powders, structural investigations have been performed. N2 adsorption method was ...