Pretraživanje
Prikaz rezultata 1-2 od 2
Influence of mechanical activation on microstructure and crystal structure of sintered MgO-TiO2 system
(Belgrade : International Institute for the Science of Sintering, 2010)
Mixtures of MgO-TiO2 were mechanically activated using high-energy planetary ball mill during 5, 10, 20, 40, 80 and 120 minutes. Sintering process was preformed in air at 1100o-1400oC for 2h. The decrease in powder’s ...
Advantages of combined sintering compared to conventional sintering of mechanically activated magnesium titanate
(Belgrade : International Institute for the Science of Sintering, 2014)
In this article, the advantages of combined sintering in comparison with the conventional one, of mechanically activated magnesium titanate ceramic were investigated. The stoichiometric mixtures of MgO and TiO2 were ...