Structural analysis of Zn2TiO4 doped with MgO
(Springer, 2009)
The starting mixtures of ZnO, TiO2, and MgO (0, 1.25, and 2.5 wt.%) powders are mechanically activated in a high-energy planetary mill for 15 min and then sintered between 800 and 1100°C for 2 h. The influence of MgO ...
Sintering of mechanically activated Zno-TiO 2 powders
(Springer, 2008)
Zinc oxide and titanium dioxide powders mixed in an equimolar ratio are mechanically activated in a planetary ball mill and sintered under nonisothermal and isothermal conditions. Nonisothermal sintering is studied using ...
Analysis of nonisothermal sintering of zinc-titanate ceramics doped with MgO
(Springer, 2008)
The aim of this work is to analyze nonisothermal sintering of zinc titanate ceramics doped with MgO obtained by mechanical activation. Mixtures of ZnO, TiO 2, and MgO (0, 1.25, and 2.5%) are mechanically activated for 15 ...
Influence of mechanical activation on electrical properties of barium–zinc–titanate ceramics sintered at 1100°C
(Springer US, 2012)
Starting mixtures of BaCO3, ZnO, and TiO2 powders are mechanically activated in a planetary ball mill for various periods of time. The powders obtained are sintered isothermally at 1100°C for 120 min. Non-isothermal sintering ...