Претраживање
Приказ резултата 1-3 од 3
Structural analysis of Zn2TiO4 doped with MgO
(Springer, 2009)
The starting mixtures of ZnO, TiO2, and MgO (0, 1.25, and 2.5 wt.%) powders are mechanically activated in a high-energy planetary mill for 15 min and then sintered between 800 and 1100°C for 2 h. The influence of MgO ...
Far infrared reflectance of sintered Zn2TiO4
(Springer Science+Business Media, 2008)
Zinc-titanate ceramics were obtained by initial mechanical activation in a high-energy planetary mill for 15 min followed by sintering at temperatures 900-1100°C for 2 h. Room temperature far infrared reflectivity spectra ...
Sintering of mechanically activated Zno-TiO 2 powders
(Springer, 2008)
Zinc oxide and titanium dioxide powders mixed in an equimolar ratio are mechanically activated in a planetary ball mill and sintered under nonisothermal and isothermal conditions. Nonisothermal sintering is studied using ...