Sintering of cordierite in the presence of MoO3 and crystallization analysis
(Belgrade : International Institute for the Science of Sintering, 2014)
Cordierite (MAS) is difficult to sinter because of the very narrow sintering temperature range (1300-1400ºC). Because a low temperature process is desirable, it is necessary to find functional ads which can allow easier ...
Influence of mechanochemical activation on the sintering of cordierite ceramics in the presence of Bi2O3 as a functional additive
(Elsevier, 2012)
Due to its outstanding electrical characteristics, such as the low temperature expansion coefficient, low dielectric constant and good mechanical properties, cordierite, 2MgO⋅2Al2O3⋅ 5SiO2, is a very attractive high-temperature ...
The fractal nature approach in ceramics materials and discrete field simulation
(ETRAN, 2018)
In this paper, we present experimental data of static fractals and compare the results with theoretical analysis obtained using dynamic particle simulation. The fractal simulator presented in this manuscript is pioneer ...
Advantages of combined sintering compared to conventional sintering of mechanically activated magnesium titanate
(Belgrade : International Institute for the Science of Sintering, 2014)
In this article, the advantages of combined sintering in comparison with the conventional one, of mechanically activated magnesium titanate ceramic were investigated. The stoichiometric mixtures of MgO and TiO2 were ...
Mechanical properties and microstructure fractal analysis of refractory bauxite concrete
(Belgrade : International Institute for the Science of Sintering, 2015)
The surface topography analysis via fractals as a means of explanation of composite materials mechanical and microstructural characteristics has hardly been reported so far. This study proposes a method of fractal analysis ...
Influence of mechanical activation on electrical properties of barium–zinc–titanate ceramics sintered at 1100°C
(Springer US, 2012)
Starting mixtures of BaCO3, ZnO, and TiO2 powders are mechanically activated in a planetary ball mill for various periods of time. The powders obtained are sintered isothermally at 1100°C for 120 min. Non-isothermal sintering ...
Influence of nitrogen and air atmosphere during thermal treatment on micro and nano sized powders and sintered TiO2 specimens
(Science of Sintering, 2014)
The influence of air and nitrogen atmosphere during heating on TiO2 nano and micro sized powders as well as sintered polycrystalline specimens was analyzed. Sintering of TiO2 nano and micro powders in air atmosphere was ...
Isothermal sintering of barium-zinc-titanate ceramics
(Oxford : Elsevier Sci Ltd., 2011)
Mixtures of BaCO3-ZnO-TiO2 were mechanically activated using high-energy planetary ball mill during 20, 40 and 80 min. As the time of mechanical activation increased, the decrease in particle size was observed. The effect ...