Sintering of mechanically activated Zno-TiO 2 powders
(Springer, 2008)
Zinc oxide and titanium dioxide powders mixed in an equimolar ratio are mechanically activated in a planetary ball mill and sintered under nonisothermal and isothermal conditions. Nonisothermal sintering is studied using ...
Influence of mechanical activation on electrical properties of barium–zinc–titanate ceramics sintered at 1100°C
(Springer US, 2012)
Starting mixtures of BaCO3, ZnO, and TiO2 powders are mechanically activated in a planetary ball mill for various periods of time. The powders obtained are sintered isothermally at 1100°C for 120 min. Non-isothermal sintering ...
Kinetics of thermally activated processes in cordierite-based ceramics
(Springer, 2019)
Thermally activated processes in cordierite-based ceramics were investigated to determine the effect of the mechanical activation and the addition of TeO2 on kinetic and thermodynamic parameters of these processes. Using ...
Enhancing Synthesis and Sintering of Zinc Titanate Using Mechanical Activation
(Progress in Advanced Materials and Processes, 2004)
Mechanical activation and sintering are used for obtaining zinc titanate, Zn2TiO4. Starting powder mixtures of ZnO and TiO2, in the molar ratio that is in accordance with the stoichiometry ofzinc titanate Zn2TiO4, were ...
The influence of mechanical activation on the stoichiometry and defect structure of a sintered ZnO-Cr2O3 system / The influence of mechanical activation on the stoichiometry and defect structure of a sintered ZnO-Cr2O3 system
(Zurich : Trans Tech Publications, 2004)
Mixtures of starting ZnO and Cr2O3 powders in equimolar quantities were mechanically activated by grinding using a high energy vibro-mill for 0, 40 and 80 minutes. Qualitative X-ray diffraction analysis made after sintering ...
Effect of mechanical activation on carbothermal synthesis and densification of ZrC
(Elsevier BV, 2023)
Zirconium carbide ceramics were prepared by carbothermal reduction of ZrO2 and C that were mixed by high-energy ball milling. Powders were milled for times from 0 to 120 min in air. As milling time increased, the surface ...
Nanomechanical properties of PVDF–ZnO polymer nanocomposite
(Elsevier BV, 2023)
Poly(vinylidenefluoride)–ZnO (PVDF–ZnO) nanocomposites with mechanically activated ZnO nanoparticle fillers were investigated using thermal and mechanical analysis and AFM and PFM. Differential scanning calorimetry (DSC) ...