Pretraživanje
Prikaz rezultata 1-1 od 1
Dilatometric Analysis of Mechanically Activated SrTiO3 Powder
(Belgrade : Serbian Ceramic Society, 2013)
Strontium-titanate powder was mechanically activated in a planetary ball mill for 0, 5, 10, 30, 60, 90 and 120 minutes. Non-isothermal sintering of non-activated and activated SrTiO3 powder samples in the temperature ...