Isothermal sintering of mechanically activated MT ceramics
(Kiev, 2009)
The aim of this work was to analyze influence of mechanical activation on MgO-TiO2 system. Mixtures of MgO-TiO2 were mechanically activated for 0, 5, 10, 20, 40, 80 and 120 minutes in a planetary ball mill and after that ...
Influence of mechanical activation on MgO-TiO2 system
(Belgrade : Institute of Technical Sciences of SASA, 2008)
In this paper the influence of mechanical activation on MgO-TiO2 system has been investigated. Mixtures of MgO-TiO2 were mechanically activated using high-energy planetary ball mill during 0, 5, 10, 20, 40, 80 and 120 ...
Phase Formation at the Sintering of Sa, Zn, Ti Oxides
(Kiev, 2009)
Complex compounds with oxide phases of Ba, 2n, and 11 are widely used in instrument engineering. It is also important to find such production routes for ceramics, which provide their stable structure and properties. Phase ...
Influence of mechanical activation on BaO-ZnO-TiO2 system
(Belgrade : Institute of Technical Sciences of SASA, 2008)
The influence of mechanical activation on BaO-ZnO-TiO2 sistem was observed. Mixtures of BaO-ZnO-TiO2 were mechanically activated using high-energy planetary ball mill during 0,5, 10, 20, 40 and 80 minutes. XRD analyses ...
Primena Ramanove spektroskopije u proučavanju mehaničke aktivacije BaTiO3
(Beograd : Institut tehničkih nauka SANU, 2006)
U ovom radu su ispitivane strukturne promene BaTiO3 tokom mehaničke aktivacije. Kao početni prah, korišćen je BaTiO3 (Aldrich) prah čistoće 99.9%. Mehanička aktivacija ovog praha izvršena je mlevenjem u visokoenergetskom ...
Enhancing Synthesis and Sintering of Zinc Titanate Using Mechanical Activation
(Progress in Advanced Materials and Processes, 2004)
Mechanical activation and sintering are used for obtaining zinc titanate, Zn2TiO4. Starting powder mixtures of ZnO and TiO2, in the molar ratio that is in accordance with the stoichiometry ofzinc titanate Zn2TiO4, were ...
The influence of mechanical activation on the stoichiometry and defect structure of a sintered ZnO-Cr2O3 system / The influence of mechanical activation on the stoichiometry and defect structure of a sintered ZnO-Cr2O3 system
(Zurich : Trans Tech Publications, 2004)
Mixtures of starting ZnO and Cr2O3 powders in equimolar quantities were mechanically activated by grinding using a high energy vibro-mill for 0, 40 and 80 minutes. Qualitative X-ray diffraction analysis made after sintering ...