Influence of mechanical activation on microstructure and crystal structure of sintered MgO-TiO2 system
(Belgrade : International Institute for the Science of Sintering, 2010)
Mixtures of MgO-TiO2 were mechanically activated using high-energy planetary ball mill during 5, 10, 20, 40, 80 and 120 minutes. Sintering process was preformed in air at 1100o-1400oC for 2h. The decrease in powder’s ...
Synthesis of barium-zinc-titanate ceramics
(Belgrade : International Institute for the Science of Sintering, 2012)
Mixtures of BaCO3, ZnO and TiO2 powders, with molar ratio of 1:2:4, were mechanically activated for 20, 40 and minutes in a planetary ball mill. The resulting powders were compacted into pellets and isothermally sintered ...