Претраживање
Приказ резултата 1-2 од 2
Characterisation of Mn0.63Zn0.37Fe2O4 powders after intensive milling and subsequent thermal treatment
(Science of Sintering, 2017)
Commercial Mn-Zn powder (Mn0.63Zn0.37Fe2O4, 93 wt. % and Fe2O3 7 wt. %) was milled 0.5, 1, 2 and 4 hours in a planetary ball mill. The goal was to observe intensive milling influences on oxidation and reduction processes ...
Influence of starting powder milling on magnetic properties of Mn-Zn ferrite
(Novi Sad : Faculty of Technology, University of Novi Sad, 2017)
In this paper, the influence of additional sieving and milling of starting industrial Mn-Zn powders on magnetic properties was investigated. The starting powder was milled for 60 minutes, followed by sieving through 325 ...