Approximation of material behaviour of PLLA polymer in HAp/PLLA biocomposite material using nanoindentation and finite element method
(Savez inženjera metalurgije Srbije, Beograd, 2007)
In this work, a combination of nanoindentation experiment and finite element modeling is proposed in order to obtain approximate material behavior of PLLA polymer in hydroxyapatite (HAp)/poly-L-lactide (PLLA) composite. ...
Micromechanical properties of a hydroxyapatite/poly-L-lactide biocomposite using nanoindentation and modulus mapping
(Oxford : Elsevier Sci Ltd., 2007)
Biocomposites with ceramic fillers and polymer matrix are becoming attractive materials for bone tissue replacements. Nanoindentation has been used to locally characterize the surface mechanical properties of the ...