The Influence of Synthesis Parameters and Heat Effect on Magnetic Properties of Powder System FexOy - BaTiO3
(Belgrade : Serbian Ceramic Society, 2015)
Powder mixture of 60 mass % of iron (Fe) and 40 mass % of barium titanate (BaTiO3) has been activated in planetary mill for 100, 120, 150, 180, 210 and 240 min in the air. During the activation the iron powder transits ...
Synthesis of BaFe12O19-BaTiO3 multiferroics by mechanical activation
(Belgrade : Serbian Ceramic Society, 2017)
A mixture of polycrystalline powders of Fe (70 % wt.) and BaTiO3 (30 % wt.) was ball-milled in a planetary mill under air atmosphere, for different time intervals: 60, 120, 180, 240, 300 and 360 min. During the mechanical ...