Electrical properties of isothermally sintered cordierite-based ceramics as function of sintering and activation time / Električna svojstva izotermski sinterovane keramike na bazi kordierita kao funkcija vremena sinterovanja i aktivacije
(Beograd : Savez mašinskih i elektrotehničkih inženjera i tehničara Srbije - SMEITS, 2021)
The mechanical activation of the starting mixtures of cordierite (2MgO*2Al2O3*5SiO2) with 5.00 mass % TiO2 was performed in a high energy ball mill during 10-80 min. The applied compaction pressure before the sintering ...
Influence of sintering time on density properties and SEM analysis of cordierite-based ceramics / Uticaj vremena sinterovanja na gustinu i SEM analiza kordijeritne keramike
(Beograd : Savez mašinskih i elektrotehničkih inženjera i tehničara Srbije - SMEITS, 2021)
The mechanical activation of the starting mixtures of cordierite (2MgO*2Al2O3*5SiO2) with 5.00 mass % TiO2 was performed in a high energy ball mill during 10-80 min. The applied compaction pressure before the sintering ...
Electronic Properties of BZT Nano-Ceramic Grades at Low Frequency Region
(Belgrade : Serbian Ceramic Society, 2021)
Barium zirconium titanate ceramics were prepared using solid state reactions of BaCO3, TiO2 and ZrO2 at elevated temperatures. The prepared BZT was mechanically activated in the planetary ball mill from 0-120 min to achieve ...
Characterization of mechanically activated ZrO2-C powder mixtures
(Belgrade : University of Belgrade - Faculty of Mechanical Engineering, 2023)
Mechanical activation represents a very useful technique for powder processing prior to sintering process. First of all, it makes powders homogenized, leads to attrition of powder particles, and makes powder mixtures more ...
Effect of mechanical activation on carbothermal synthesis and densification of ZrC
(Elsevier BV, 2023)
Zirconium carbide ceramics were prepared by carbothermal reduction of ZrO2 and C that were mixed by high-energy ball milling. Powders were milled for times from 0 to 120 min in air. As milling time increased, the surface ...