Influence of mechanical activation on microstructure and crystal structure of sintered MgO-TiO2 system
(Belgrade : International Institute for the Science of Sintering, 2010)
Mixtures of MgO-TiO2 were mechanically activated using high-energy planetary ball mill during 5, 10, 20, 40, 80 and 120 minutes. Sintering process was preformed in air at 1100o-1400oC for 2h. The decrease in powder’s ...
Barium-zinc-titanate ceramics
(Kiev : National Academy of Sciences of Ukraine (NASU); Frantsevych Institute for Problems of Materials Science of NASU; National Technical University of Ukraine "KPI"; Ukrainian Materials Science Society; INTEM LTD, 2010)
Starting mixtures of BaCO3, ZnO and TiO2 powders were mechanically activated in a planetary ball mill for various periods of time. The powders obtained were sintered nonisothermally to temperatures between 1100 and 1300°C ...
Structural and Electrical Properties of Barium-Zinc-Titanate Ceramics Sintered at 1300°C
(2010)
Poster presented at the 12th Annual Conference of the Materials Research Society of Serbia - YUCOMAT 2010, Herceg Novi, Montenegro, September 6–10, 2010.