Reaction sintering of the 2ZnO-TiO2 system
(Belgrade : International Institute for the Science of Sintering, 2007)
Sintering kinetics of the mechanically activated ZnO-TiO2 system was studied. Mixtures of ZnO and TiO2 powders were mechanically activated using a high-energy ball mill for different time intervals from 0 to 300 minutes. ...
Investigation of zinc stannate synthesis using photoacoustic spectroscopy
(Belgrade : International Institute for the Science of Sintering, 2007)
Mixtures of ZnO and SnO2 powders, with molar ratio of 2:1, were mechanically activated for 40, 80 and 160 minutes in a planetary ball mill. The resulting powders were compacted into pellets and non-isothermally sintered ...
Changes of Structural, Optical and Electrical Properties of Nickel-Manganite Ceramics Induced by Additional Mechanical Activation
(2007)
Poster presented at the 10th International Conference and Exhibition of the European Ceramic Society, Berlin, June 17-21, 2007
Intrinsic resistivity of sintered nickel manganite vs. powder activation time and density
(2007)
Poster presented at the conference Fizika i tehnologija materijala (Physics and Technology of Materials), FITEM '07, Čačak, Serbia, August 6-8, 2007.
Ispitivanje sinterovane cink-kalaj-oksidne keramike fotoakustičnom spektroskopijom
(Beograd : Savez hemijskih inženjera, 2007)
Prahovi ZnO i SnO2 pomešani u molamom odnosu 2:1 mehanički su aktivi- rani u planetamim mlinu sa kuglama u intervalu od 10 do 160 minuta. Do- bijene smeše presovane su i izotermski sinterovane na 1300 °C, dva sata. Uzorci ...