Synthesis of spherical beta-silicon carbide particles by ultrasonic spray pyrolysis
Samo za registrovane korisnike
1996
Članak u časopisu (Objavljena verzija)
Metapodaci
Prikaz svih podataka o dokumentuApstrakt
Fine agglomerate-free spherical beta-SiC powder was synthesized from a dispersion of colloidal silica, saccharose, and boric acid, by means of an ultrasonic spray pyrolysis method, Droplets of 2.2 mu m were formed with an aerosol generator, operated at 2.5 MHz, and carried into a reaction furnace at 900 degrees C with argon, Spherical X-ray amorphous gel particles of 1.1 mu m were obtained, beta-SiC particles with a mean diameter of 0.79 mu m and spherical shape resulted when the SiC gel precursor particles were heated at 1500 degrees C in argon.
Izvor:
Journal of the American Ceramic Society, 1996, 79, 8, 2215-2217
DOI: 10.1111/j.1151-2916.1996.tb08964.x
ISSN: 0002-7820 (Print)
WoS: A1996VC61300036
Scopus: 2-s2.0-0030214054
Institucija/grupa
Институт техничких наука САНУ / Institute of Technical Sciences of SASATY - JOUR AU - Cerović, L. S. AU - Milonjić, Slobodan AU - Živković, L. V. AU - Uskoković, Dragan PY - 1996 UR - https://dais.sanu.ac.rs/123456789/3347 AB - Fine agglomerate-free spherical beta-SiC powder was synthesized from a dispersion of colloidal silica, saccharose, and boric acid, by means of an ultrasonic spray pyrolysis method, Droplets of 2.2 mu m were formed with an aerosol generator, operated at 2.5 MHz, and carried into a reaction furnace at 900 degrees C with argon, Spherical X-ray amorphous gel particles of 1.1 mu m were obtained, beta-SiC particles with a mean diameter of 0.79 mu m and spherical shape resulted when the SiC gel precursor particles were heated at 1500 degrees C in argon. T2 - Journal of the American Ceramic Society T1 - Synthesis of spherical beta-silicon carbide particles by ultrasonic spray pyrolysis SP - 2215 EP - 2217 VL - 79 IS - 8 DO - 10.1111/j.1151-2916.1996.tb08964.x UR - https://hdl.handle.net/21.15107/rcub_dais_3347 ER -
@article{ author = "Cerović, L. S. and Milonjić, Slobodan and Živković, L. V. and Uskoković, Dragan", year = "1996", abstract = "Fine agglomerate-free spherical beta-SiC powder was synthesized from a dispersion of colloidal silica, saccharose, and boric acid, by means of an ultrasonic spray pyrolysis method, Droplets of 2.2 mu m were formed with an aerosol generator, operated at 2.5 MHz, and carried into a reaction furnace at 900 degrees C with argon, Spherical X-ray amorphous gel particles of 1.1 mu m were obtained, beta-SiC particles with a mean diameter of 0.79 mu m and spherical shape resulted when the SiC gel precursor particles were heated at 1500 degrees C in argon.", journal = "Journal of the American Ceramic Society", title = "Synthesis of spherical beta-silicon carbide particles by ultrasonic spray pyrolysis", pages = "2215-2217", volume = "79", number = "8", doi = "10.1111/j.1151-2916.1996.tb08964.x", url = "https://hdl.handle.net/21.15107/rcub_dais_3347" }
Cerović, L. S., Milonjić, S., Živković, L. V.,& Uskoković, D.. (1996). Synthesis of spherical beta-silicon carbide particles by ultrasonic spray pyrolysis. in Journal of the American Ceramic Society, 79(8), 2215-2217. https://doi.org/10.1111/j.1151-2916.1996.tb08964.x https://hdl.handle.net/21.15107/rcub_dais_3347
Cerović LS, Milonjić S, Živković LV, Uskoković D. Synthesis of spherical beta-silicon carbide particles by ultrasonic spray pyrolysis. in Journal of the American Ceramic Society. 1996;79(8):2215-2217. doi:10.1111/j.1151-2916.1996.tb08964.x https://hdl.handle.net/21.15107/rcub_dais_3347 .
Cerović, L. S., Milonjić, Slobodan, Živković, L. V., Uskoković, Dragan, "Synthesis of spherical beta-silicon carbide particles by ultrasonic spray pyrolysis" in Journal of the American Ceramic Society, 79, no. 8 (1996):2215-2217, https://doi.org/10.1111/j.1151-2916.1996.tb08964.x ., https://hdl.handle.net/21.15107/rcub_dais_3347 .