Sintering of cordierite in the presence of MoO3 and crystallization analysis
(Belgrade : International Institute for the Science of Sintering, 2014)
Cordierite (MAS) is difficult to sinter because of the very narrow sintering temperature range (1300-1400ºC). Because a low temperature process is desirable, it is necessary to find functional ads which can allow easier ...
Advantages of combined sintering compared to conventional sintering of mechanically activated magnesium titanate
(Belgrade : International Institute for the Science of Sintering, 2014)
In this article, the advantages of combined sintering in comparison with the conventional one, of mechanically activated magnesium titanate ceramic were investigated. The stoichiometric mixtures of MgO and TiO2 were ...