Sintering of fly ash based composites with zeolite and bentonite addition for application in construction materials
(International Institute for the Science of Sintering, 2017)
Due to pozzolanic characteristics, fly ash is commonly used as a cement replacement in construction composites. Addition of natural clays with sorption ability (i.e. zeolite and bentonite) in to the fly ash based construction ...
Influence of nitrogen and air atmosphere during thermal treatment on micro and nano sized powders and sintered TiO2 specimens
(Belgrade : International Institute for the Science of Sintering, 2014)
The influence of air and nitrogen atmosphere during heating on TiO2 nano and micro sized powders as well as sintered polycrystalline specimens was analyzed. Sintering of TiO2 nano and micro powders in air atmosphere was ...
The influence of mechanical activation on sintering process of BaCO3-SrCO3-TiO2 system
(Belgrade : International Institute for the Science of Sintering, 2012)
In this article the influence of mechanical activation on sintering process of bariumstrontium-titanate ceramics has been investigated. Both non-activated and mixtures treated in a planetary ball mill for 5, 10, 20, 40, ...
Electrical properties of magnesium titanate ceramics post-sintered by hot isostatic pressing
(Belgrade : International Institute for the Science of Sintering, 2017)
Post-sintering of magnesium titanate ceramics by hot isostatic pressing (HIP) in an oxygen-free atmosphere significantly alters various electrical properties of the product. In particular, the sintered material becomes a ...
Intrinsic resistivity of sintered Nickel Manganite vs. powder activation time and density
(Belgrade : International Institute for the Science of Sintering, 2008)
In this work the DC resistivity of sintered nickel manganite NiMn2O4 (NTC thermistor material) was studied as a function of additional powder activation time in a planetary ball mill (0, 5, 15, 30, 45 and 60 min). The ...
ZnTiO3 ceramic nanopowder microstructure changes during compaction
(Belgrade : International Institute for the Science of Sintering, 2013)
ZnTiO3 nanopowder as a constitutive component in compact production was primarily characterized. Scanning electron micrographs of as received powder were recorded. Mercury porosimetry and nitrogen adsorption were also ...
Mechanical activation as sintering pre-treatment of talc for steatite ceramics
(Belgrade : Interenational Institute for the Science of Sintering, 2014)
The effect of vibratory mill induced mechanical activation on the change of the particle size, crystallinity and the phase transformations of the minerals present in the activated material, was studied with the purpose of ...
Study of dielectric behavior and electrical properties of hematite α-Fe2O3 doped with Zn
(Belgrade : International Institute for the Science of Sintering, 2012)
The effects of Zn-doping on the dielectric behavior and electrical properties of bulk α-Fe2O3 have been studied. X-ray diffraction analysis revealed the presence of two phases in all samples: hematite and spinel ZnFe2O4, ...
Structural and electrical properties of Ti doped α-Fe2O3
(Belgrade : International Institute for the Science of Sintering, 2013)
In this work we have analyzed the effects of Ti doping on structural and electrical properties of α-Fe2O3. When the amount of added Ti (5 wt.%TiO2) was within the solubility degree and XRD, SEM and EDS analysis revealed a ...
Electronic ceramic structure within the Voronoi cells model and microstructure fractals contacts surfaces new frontier applications
(Belgrade : International Institute for the Science of Sintering, 2013)
In this study, in order to establish grain shapes of sintered ceramics, new approach on correlation between microstructure and doped BaTiO3 -ceramics properties based, on Voronoi model and mathematical statistics calculations ...