Influence of mechanical activation on functional properties of barium hexaferrite ceramics
(Elsevier, 2018)
Barium hexaferrite ceramics were prepared using mechanically activated mixtures of iron and barium titanate. The 60:40 mass% Fe:BaTiO3 powder mixtures were mechanically activated for different times (100–240 min) and ...
Processing and properties of dense cordierite ceramics obtained through solid-state reaction and pressure-less sintering
(Taylor and Francis, 2019)
Sintering of pure cordierite 2MgO:2Al2O3:5SiO2, and cordierite with the addition of 5 mass % TeO2 was studied. Green bodies were prepared from powder mixtures mechanically activated in a high-energy planetary mill, shaped ...
Reheating of zinc-titanate sintered specimens
(Belgrade : International Institute for the Science of Sintering, 2015)
The scope of this work was observing dimensional and heat transfer changes in ZnTiO3 samples during heating in nitrogen and air atmosphere. Interactions of bulk specimens with gaseous surrounding induce microstructure ...
Adsorption capacity of wollastonite based adsorbents with porous structure controlled with different progeny agents
(Belgrade : Serbian Ceramic Society, 2016)
Porous wollastonite (WL) based adsorbents were fabricated by a pressureless sintering process by using low molecular weight poly(methyl methacrylate) (PMMA), nanocellulose (NC) and yeast as the pore forming agents. WL based ...
The influence of mechanical activation on the electrical properties of Ba0.77Sr0.23TiO3 ceramics
(Elsevier, 2014)
Ferroelectric barium strontium titanate (Ba0.77Sr0.23TiO3), BST, was prepared by solid-state reactions using as the starting compounds powder of barium carbonate (BaCO3), strontium carbonate (SrCO3) and titanium dioxide ...
Structural and electrical properties of sintered Fe2O3/TiO2 nanopowder mixtures
(Elsevier, 2014)
Starting nanopowders of TiO2 (anatase 99.7%) and α-Fe2O3 (hematite) were mixed in the weight ratios 60:40 and 40:60. Green samples were sintered in the temperature range 750–1250 °C in air. Structural, morphological and ...
Nanostructured Fe2O3/TiO2 thick films: Analysis of structural and electronic properties
(Elsevier, 2015)
Thick films using starting nanopowders of TiO2 (anatase 99.7%) and α-Fe2O3 (hematite) mixed in the weight ratios 60:40 and 40:60 for thick film paste were fabricated by screen printing technology on an alumina substrate. ...
Assessment of intensive grinding effects on alumina as refractory compound: Acceleration of γ to α phase transformation mechanism
(Elsevier, 2014)
In this study, the feasibility of alumina phase transition enhancement by mechanical activation was conducted. It was showed that the milling environment plays an important role on the physical, chemical and thermal behavior ...
Fractal nature Heywang model contribution and BaTiO3-ceramics semiconducting phenomena
(Belgrade : Serbian Ceramic Society, 2018)
Well known material with ferroelectric properties, BaTiO3-ceramics, have many advanced applications. Fractal approach in analyzing of these structures can be one of the solution for investigation of morphology. It is known ...
The influence of powder characteristics on two-step sintering behavior of hydroxyapatite
(Belgrade : Institute of Technical Sciences of SASA, 2010)
Fabrication of full dense ceramic materials on the basis of hydroxyapatite (HAp) and biphasic calcium phosphate (BCP) with controllable microstructural and compositional characteristics attracts considerable efforts. Various ...