Search
Now showing items 21-30 of 62
Isothermal sintering of mechanically activated MT ceramics
(Kiev, 2009)
The aim of this work was to analyze influence of mechanical activation on MgO-TiO2 system. Mixtures of MgO-TiO2 were mechanically activated for 0, 5, 10, 20, 40, 80 and 120 minutes in a planetary ball mill and after that ...
Characterization of electrochemically synthesized pani on graphite electrode for potential use in electrochemical power sources / Elektrohemijska sinteza i karakterizacija elektrode od polianilina za potencijalnu upotrebu u elektrohemijskim izvorima energije
(Engineering Society for Corrosion, Belgrade, Serbia, 2009)
Polyaniline (PANI) on graphite electrode was synthesized electrochemically under galvanostatic condition at current density of 2.0 mA cm-2 from aqueous solution of 1.0 moldm-3 HCl and 0.25 mol dm-3 aniline monomer. ...
Strukturne, morfološke i funkcionalne karakteristike nanostrukturnih oksida retkih zemalja dobijenih aerosol sintezom
(Belgrade : University of Belgrade, Faculty of Technollogy and Metallurgy, 2009)
Dobijanje ultrafinih, sferičnih, fosforescentnih čestica sa homogenom raspodelom komponenata i faza je od posebnog značaja za materijale sa primenom u savremenim optoelektronskim uređajima. Reakcija u disperznom sistemu ...
Formation of magnesium titanates
(Springer, 2009)
The paper examines the phase formation in the mechanochemical treatment and subsequent annealing of TiO 2 and MgO mixtures. It is established that the MgTiO 3 phase forms during annealing of the above powder mixtures at ...
Effect of chemisorbed carbon monoxide on Pt/C electrode on the mechanism of the hydrogen oxidation reaction
(Elsevier, 2009)
The influence of poisoning of Pt catalyst by CO on the kinetics and mechanism of H2 oxidation reaction (HOR) at Pt/C electrode in 0.5 mol dm-3 HClO4, saturated with H2 containing 100 ppm CO, was examined with rotating disc ...
Influence of MgO addition on the synthesis and electrical properties of sintered zinc-titanate ceramics
(Elsevier, 2009)
Starting mixtures of ZnO, TiO2 and MgO (0, 1.25 and 2.5 wt.% MgO) powders were mechanically activated for 15 min in a planetary ball mill. The powders obtained were sintered non-isothermally to temperatures between 800 and ...
Structural analysis of Zn2TiO4 doped with MgO
(Springer, 2009)
The starting mixtures of ZnO, TiO2, and MgO (0, 1.25, and 2.5 wt.%) powders are mechanically activated in a high-energy planetary mill for 15 min and then sintered between 800 and 1100°C for 2 h. The influence of MgO ...
Isothermal sintering of BZT ceramics
(Kiev, 2009)
Starting mixtures of BaCO3 •ZnO and Ti02 were mechanically activated for 0,5, 10,20.40 and 80 minutes in a planetary ball mill. The powders obtained were sintered isothermally to temperatures between 1000 and 1300 °C. The ...
Citrate-based zinc-polyaniline secondary cell: Part I: Optimization of the citrate/chloride electrolyte
(Springer, 2009)
Electrochemical behavior of zinc and thin polyaniline (PANI) electrodes in citrate/chloride-contained electrolyte has been investigated by the means of electrolyte composition optimization. Electrolyte contained 0.8 M ...
Characterization of electrochemically synthesized PANI on graphite electrode for potential use in electrochemical power sources
(Materials Chemistry and Physics, 2009)
Polyaniline (PANI) on graphite electrode was synthesized electrochemically under galvanostatic condition at current density of 2.0 mA cm-2 from aqueous solution of 1.0 mol dm-3 HCl and 0.25 mol dm-3 aniline monomer. ...