The effect of Hot Isostatic Pressing on the MT sample densities
(Belgrade : Serbian Ceramic Society, 2015)
Mechanically activated powders (0, 10, 40, 80 and 160 minutes) were formed by isostatic pressure 300 MPa to cylindrical green bodies (φ 12 mm). First set of samples was sintered at 1300°C for 30 min in air (heating rate ...
Kinetics of Mechanically Activated TiO2-based Oxides Followed by DTA
(Belgrade : Serbian Ceramic Society, 2012)
TiO2-based materials are widely used in production of ceramic capacitors and semiconductors. The conventional method of ceramics synthesis relies on the solid-state reaction between TiO2 and other compounds (BaCO3, BaO, ...