Претраживање
Приказ резултата 1-3 од 3
Structural analysis of Zn2TiO4 doped with MgO
(Springer, 2009)
The starting mixtures of ZnO, TiO2, and MgO (0, 1.25, and 2.5 wt.%) powders are mechanically activated in a high-energy planetary mill for 15 min and then sintered between 800 and 1100°C for 2 h. The influence of MgO ...
Influence of MgO addition on the synthesis and electrical properties of sintered zinc-titanate ceramics
(Elsevier, 2009)
Starting mixtures of ZnO, TiO2 and MgO (0, 1.25 and 2.5 wt.% MgO) powders were mechanically activated for 15 min in a planetary ball mill. The powders obtained were sintered non-isothermally to temperatures between 800 and ...
Mechanochemical synthesis and electrical conductivity of nanocrystalline δ-Bi2O3 stabilized by HfO2 and ZrO2
(Belgrade : Serbian Chemical Society, 2009)
A powder mixture of α-Bi2O3 and HfO2, in the molar ratio 2:3, was mechanochemically treated in a planetary ball mill under air, using zirconium oxide vials and balls as the milling medium. After 50 h of milling, the ...