The effect of mechanical activation on synthesis and properties of MgAl2O4 ceramics
(Elsevier, 2019)
Magnesium aluminate, MgAl2O4 and other alumina-based spinels are ceramics with high hardness, high melting point and mechanical strenght. Spinels can also be used as dielectrics in microwave applications. The goal of this ...
Structural analysis of Zn2TiO4 doped with MgO
(Springer, 2009)
The starting mixtures of ZnO, TiO2, and MgO (0, 1.25, and 2.5 wt.%) powders are mechanically activated in a high-energy planetary mill for 15 min and then sintered between 800 and 1100°C for 2 h. The influence of MgO ...
Investigation of thermally induced processes in corundum refractory concretes with addition of fly ash
(Springer Netherlands, 2015)
The effects that the fly ash addition has on the behavior of thermally resistant corundum concrete were discussed. Experimental program implied production of two refractory composites: "referent" concrete from 20 % of ...
Influence of mechanochemical activation on the sintering of cordierite ceramics in the presence of Bi2O3 as a functional additive
(Elsevier, 2012)
Due to its outstanding electrical characteristics, such as the low temperature expansion coefficient, low dielectric constant and good mechanical properties, cordierite, 2MgO⋅2Al2O3⋅ 5SiO2, is a very attractive high-temperature ...
Microwave Electro Ceramic Based on Magnesium Titanate Compounds
(Paris : Atlantis Press, 2017)
The intensive progress in electronics, especially telecommunication and mobile phone in 1990s, was the main driving force for the extensive research and development of microwave ceramics. These materials are often used in ...
Mechanically activated coal ash as refractory bauxite shotcrete microfiller: Thermal interactions mechanism investigation
(Elsevier, 2014)
A growing demand for refractory castables with advanced properties has given rise to a continuous technological evolution and highlighted the necessity for secondary raw materials reapplication even in refractory industry. ...
Influence of mechanical activation on electrical properties of barium–zinc–titanate ceramics sintered at 1100°C
(Springer US, 2012)
Starting mixtures of BaCO3, ZnO, and TiO2 powders are mechanically activated in a planetary ball mill for various periods of time. The powders obtained are sintered isothermally at 1100°C for 120 min. Non-isothermal sintering ...
The influence of mechanical activation on the electrical properties of Ba0.77Sr0.23TiO3 ceramics
(Elsevier, 2014)
Ferroelectric barium strontium titanate (Ba0.77Sr0.23TiO3), BST, was prepared by solid-state reactions using as the starting compounds powder of barium carbonate (BaCO3), strontium carbonate (SrCO3) and titanium dioxide ...
Sintering of Zinc-Titanate
(Atlantis Press, 2016)
Sintering kinetics of the mechanically activated ZnO-TiO2 system was studied. Mixtures of ZnO and TiO2 powders were mechanically activated using a high-energy ball mill for different time intervals from 0 to 300 min. Formal ...
Sintering of mechanically activated Zno-TiO 2 powders
(Springer, 2008)
Zinc oxide and titanium dioxide powders mixed in an equimolar ratio are mechanically activated in a planetary ball mill and sintered under nonisothermal and isothermal conditions. Nonisothermal sintering is studied using ...