Претраживање
Приказ резултата 1-2 од 2
Morphology investigation of mechanically activated ZnO-SnO2 system
(Elsevier, 2008)
Powder mixtures of zinc oxide and tin oxide in the molar ratio, ZnO:SnO2 = 2:1, were mechanically activated in a planetary ball mill in the time intervals of 0-160 min. The adsorption-desorption isotherms, specific surface ...
Analysis of nonisothermal sintering of zinc-titanate ceramics doped with MgO
(Springer, 2008)
The aim of this work is to analyze nonisothermal sintering of zinc titanate ceramics doped with MgO obtained by mechanical activation. Mixtures of ZnO, TiO 2, and MgO (0, 1.25, and 2.5%) are mechanically activated for 15 ...