Synthesis of BaTiO3 from a mechanically activated BaCO 3-TiO2 system
(Belgrade : International Institute for the Science of Sintering, 2008)
In this article the solid state reaction of BaTiO3 formation from a mechanically activated BaCO3-TiO2 system has been investigated. An equimolar mixture of BaCO3 and TiO2 powders was activated in a planetary ball mill in ...
Investigation of zinc stannate synthesis using photoacoustic spectroscopy
(Belgrade : International Institute for the Science of Sintering, 2007)
Mixtures of ZnO and SnO2 powders, with molar ratio of 2:1, were mechanically activated for 40, 80 and 160 minutes in a planetary ball mill. The resulting powders were compacted into pellets and non-isothermally sintered ...
Analysis of the initial-stage sintering of mechanically activated SrTiO3
(ETRAN, 2019)
The initial-stage of sintering plays a significant role in determining the final microstructure that defines the main characteristics of electroceramics materials such as functional properties. In this article non-isothermal ...
Influence of mechanochemical activation on the sintering of cordierite ceramics in the presence of Bi2O3 as a functional additive
(Elsevier, 2012)
Due to its outstanding electrical characteristics, such as the low temperature expansion coefficient, low dielectric constant and good mechanical properties, cordierite, 2MgO⋅2Al2O3⋅ 5SiO2, is a very attractive high-temperature ...
Sintering of mechanically activated Zno-TiO 2 powders
(Springer, 2008)
Zinc oxide and titanium dioxide powders mixed in an equimolar ratio are mechanically activated in a planetary ball mill and sintered under nonisothermal and isothermal conditions. Nonisothermal sintering is studied using ...
Influence of mechanical activation on electrical properties of barium–zinc–titanate ceramics sintered at 1100°C
(Springer US, 2012)
Starting mixtures of BaCO3, ZnO, and TiO2 powders are mechanically activated in a planetary ball mill for various periods of time. The powders obtained are sintered isothermally at 1100°C for 120 min. Non-isothermal sintering ...
Ispitivanje sinterovane cink-kalaj-oksidne keramike fotoakustičnom spektroskopijom
(Beograd : Savez hemijskih inženjera, 2007)
Prahovi ZnO i SnO2 pomešani u molamom odnosu 2:1 mehanički su aktivi- rani u planetamim mlinu sa kuglama u intervalu od 10 do 160 minuta. Do- bijene smeše presovane su i izotermski sinterovane na 1300 °C, dva sata. Uzorci ...
Morphological and Structural Characterization of MgAl2O4 Spinel
(ETRAN, 2023)
Magnesium aluminate has the spinel structure along with good mechanical, chemical, and thermal properties. Magnesium aluminate has a wide range of applications including refractory ceramics, optically transparent ceramic ...