Characterization of Mechanochemically Synthesized CaO·ZnO/K2O Mixed Oxides
(Belgrade : Serbian Ceramic Society, 2012)
Room temperature ball milling of CaO and ZnO powder mixture (using molar ratio of CaO:ZnO of 1:2) with the addition of stoichiometrically required amount of water to form calcium zinc hydroxide hydrate (CaZn2(OH)6•2H2O) ...
Humidity sensing potential of iron manganite (FeMNO3)
(Budapest : [s. n.], 2019)
Though different metal oxide systems have been investigated and applied in humidity sensing as resistive or capacitive ceramic humidity sensors new materials remain the subject of much research. Iron manganite (FeMnO3) has ...
Dielectric characteristics of polymer nanocomposites based on PVDF and mechanically activated ZnO powder
(Belgrade : Serbian Ceramic Society, 2021)
ZnO powder was mechanically activated for 10 and 30 minutes in a high energy planetary ball mill, and mixed with 2 wt% PVDF solution to obtain nanocomposite films (50 μm) by casting. ZnO powder activated for 10 and 30 ...
The Influence of Synthesis Parameters and Heat Effect on Magnetic Properties of Powder System FexOy - BaTiO3
(Belgrade : Serbian Ceramic Society, 2015)
Powder mixture of 60 mass % of iron (Fe) and 40 mass % of barium titanate (BaTiO3) has been activated in planetary mill for 100, 120, 150, 180, 210 and 240 min in the air. During the activation the iron powder transits ...
Analysis of isothermal sintering of zinc-titanate doped with MgO
(Čačak : Technical Faculty, 2007)
The aim of this work was analysis of isothermal sintering of zinc titanate ceramics doped with MgO obtained by mechanical activation. Mixtures of ZnO, Ti02 and MgO (0, 1.25 and 2.5%) were mechanically activated 15 minutes ...
Dilatometric Analysis of Mechanically Activated SrTiO3 Powder
(Belgrade : Serbian Ceramic Society, 2013)
Strontium-titanate powder was mechanically activated in a planetary ball mill for 0, 5, 10, 30, 60, 90 and 120 minutes. Non-isothermal sintering of non-activated and activated SrTiO3 powder samples in the temperature ...
Influence of synthesis parameters and thermal treatment on functional properties of Fe3O4-BaTiO3 multiferroics obtained by mechanical activation
(Belgrade : Serbian Ceramic Society, 2017)
Mechanical activation of a mixture of polycrystalline powders Fe3O4 (50% wt.) and BaTiO3 (50% wt.) was performed in a planetary ball-mill, with different milling times (3 h, 6 h and 12 h). Average crystallite size determined ...
Structural characterization of mechanically activated MgO-TiO2 system
(Belgrade : Materials Research Society of Serbia, 2011)
Mixtures of MgO-TiO2 powders were mechanically activated in a planetary ball mill for time interval from 0 to 120 minutes. On thus obtained powders, structural investigations have been performed. N2 adsorption method was ...
Tailoring the microstructure of Mn-Zn ferrite to electronic properties
(Belgrade : Institute for Multidisciplinary Research, University of Belgrade, 2015)
Commercial Mn-Zn ferrite powder was milled in a planetary ball mill for 30-240 minutes. Particle size distribution in the milled powders was analyzed using a laser particle size analyzer and correlated with XRD and SEM ...
Influence of mechanical activation on BaO-ZnO-TiO2 system
(Belgrade : Institute of Technical Sciences of SASA, 2008)
The influence of mechanical activation on BaO-ZnO-TiO2 sistem was observed. Mixtures of BaO-ZnO-TiO2 were mechanically activated using high-energy planetary ball mill during 0,5, 10, 20, 40 and 80 minutes. XRD analyses ...