Structural analysis of Zn2TiO4 doped with MgO
(Springer, 2009)
The starting mixtures of ZnO, TiO2, and MgO (0, 1.25, and 2.5 wt.%) powders are mechanically activated in a high-energy planetary mill for 15 min and then sintered between 800 and 1100°C for 2 h. The influence of MgO ...
Influence of MgO addition on the synthesis and electrical properties of sintered zinc-titanate ceramics
(Elsevier, 2009)
Starting mixtures of ZnO, TiO2 and MgO (0, 1.25 and 2.5 wt.% MgO) powders were mechanically activated for 15 min in a planetary ball mill. The powders obtained were sintered non-isothermally to temperatures between 800 and ...