Претраживање
Приказ резултата 1-3 од 3
Structural analysis of Zn2TiO4 doped with MgO
(Springer, 2009)
The starting mixtures of ZnO, TiO2, and MgO (0, 1.25, and 2.5 wt.%) powders are mechanically activated in a high-energy planetary mill for 15 min and then sintered between 800 and 1100°C for 2 h. The influence of MgO ...
Sintering of mechanically activated Zno-TiO 2 powders
(Springer, 2008)
Zinc oxide and titanium dioxide powders mixed in an equimolar ratio are mechanically activated in a planetary ball mill and sintered under nonisothermal and isothermal conditions. Nonisothermal sintering is studied using ...
Enhancing Synthesis and Sintering of Zinc Titanate Using Mechanical Activation
(Progress in Advanced Materials and Processes, 2004)
Mechanical activation and sintering are used for obtaining zinc titanate, Zn2TiO4. Starting powder mixtures of ZnO and TiO2, in the molar ratio that is in accordance with the stoichiometry ofzinc titanate Zn2TiO4, were ...