Advantages of combined sintering compared to conventional sintering of mechanically activated magnesium titanate

2014
Аутори
Filipović, Suzana
Obradović, Nina

Pavlović, Vladimir B.

Kosanović, Darko

Mitrić, Miodrag

Pouchly, Vaclav
Kachlik, Martin

Maca, Karel

Чланак у часопису (Објављена верзија)
Метаподаци
Приказ свих података о документуАпстракт
In this article, the advantages of combined sintering in comparison with the conventional one, of mechanically activated magnesium titanate ceramic were investigated. The stoichiometric mixtures of MgO and TiO2 were mechano-chemically activated for 0, 10, 40, 80 and 160 minutes by ball milling and then isostatically pressed (CIP) to form green bodies. Conventional sintering was realized by heating up to 1400 oC and hold for 30 minutes in air atmosphere. Resulting ceramic samples with closed porosity were post-sintered by pressure assisted technique Hot Isostatic Pressing (HIP) at 1280 oC/3h in argon atmosphere with a pressure of 200 MPa. The best results were observed in the case of samples post-sintered by HIP, when single-phase MgTiO3 samples with relative density of 96% were prepared. [Projekat Ministarstva nauke Republike Srbije, br. OI 172057]
Кључне речи:
sintering / ceramics / magnesium titanateИзвор:
Science of Sintering, 2014, 46, 3, 283-290Издавач:
- Belgrade : International Institute for the Science of Sintering
Пројекти:
- Усмерена синтеза, структура и својства мултифункционалних материјала (RS-172057)
- Serbian Academy of Sciences and Arts, Project F-198
- European Regional Development Fund through a project CEITEC, CZ.1.05/1.1.00/02.0068
DOI: 10.2298/SOS1403283F