Advantages of combined sintering compared to conventional sintering of mechanically activated magnesium titanate

2014
Authors
Filipović, Suzana
Obradović, Nina

Pavlović, Vladimir B.

Kosanović, Darko

Mitrić, Miodrag

Pouchly, Vaclav
Kachlik, Martin

Maca, Karel

Article (Published version)
Metadata
Show full item recordAbstract
In this article, the advantages of combined sintering in comparison with the conventional one, of mechanically activated magnesium titanate ceramic were investigated. The stoichiometric mixtures of MgO and TiO2 were mechano-chemically activated for 0, 10, 40, 80 and 160 minutes by ball milling and then isostatically pressed (CIP) to form green bodies. Conventional sintering was realized by heating up to 1400 oC and hold for 30 minutes in air atmosphere. Resulting ceramic samples with closed porosity were post-sintered by pressure assisted technique Hot Isostatic Pressing (HIP) at 1280 oC/3h in argon atmosphere with a pressure of 200 MPa. The best results were observed in the case of samples post-sintered by HIP, when single-phase MgTiO3 samples with relative density of 96% were prepared. [Projekat Ministarstva nauke Republike Srbije, br. OI 172057]
Keywords:
sintering / ceramics / magnesium titanateSource:
Science of Sintering, 2014, 46, 3, 283-290Publisher:
- Belgrade : International Institute for the Science of Sintering
Projects:
- Directed synthesis, structure and properties of multifunctional materials (RS-172057)
- Serbian Academy of Sciences and Arts, Project F-198
- European Regional Development Fund through a project CEITEC, CZ.1.05/1.1.00/02.0068
DOI: 10.2298/SOS1403283F
ISSN: 0350-820X (Print); 1820-7413 (Online)