The effect of temperature and frequency on magnetic properties of the Fe81B13Si4C2 amorphous alloy

Đukić, S.; Maričić, V.; Kalezić Glišović, Aleksandra; Ribić Zelenović, Lenka; Ranđić, Siniša; Mitrović, Nebojša; Obradović, Nina

(Belgrade : ETRAN, 2011)

TY  - JOUR
AU  - Đukić, S.
AU  - Maričić, V.
AU  - Kalezić Glišović, Aleksandra
AU  - Ribić Zelenović, Lenka
AU  - Ranđić, Siniša
AU  - Mitrović, Nebojša
AU  - Obradović, Nina
PY  - 2011
UR  - https://dais.sanu.ac.rs/123456789/16291
AB  - In this study it was investigated influence of temperature and frequency on permeability, coercivity and power loses of Fe81B13Si4C2 amorphous alloy. Magnetic permeability measurements performed in nonisothermal and isothermal conditions was confirmed that efficient structural relaxation was occurred at temperature of 663 K. This process was performed in two steps, the first one is kinetic and the second one is diffuse. Activation energies of these processes are: Ea1 = 52.02 kJ/mol for kinetic and Ea2 = 106.9 kJ/mol for diffuse. It was shown that after annealing at 663 K coercivity decrease about 30% and therefore substantial reduction in power loses was attained. Investigated amorphous alloy satisfied the criteria for signal processing devices that work in mean frequency domain.
PB  - Belgrade : ETRAN
T2  - Science of Sintering
T1  - The effect of temperature and frequency on magnetic properties of the Fe81B13Si4C2 amorphous alloy
SP  - 175
EP  - 182
VL  - 43
IS  - 2
DO  - 10.2298/SOS1102175D
UR  - https://hdl.handle.net/21.15107/rcub_dais_16291
ER  - 
@article{
author = "Đukić, S. and Maričić, V. and Kalezić Glišović, Aleksandra and Ribić Zelenović, Lenka and Ranđić, Siniša and Mitrović, Nebojša and Obradović, Nina",
year = "2011",
abstract = "In this study it was investigated influence of temperature and frequency on permeability, coercivity and power loses of Fe81B13Si4C2 amorphous alloy. Magnetic permeability measurements performed in nonisothermal and isothermal conditions was confirmed that efficient structural relaxation was occurred at temperature of 663 K. This process was performed in two steps, the first one is kinetic and the second one is diffuse. Activation energies of these processes are: Ea1 = 52.02 kJ/mol for kinetic and Ea2 = 106.9 kJ/mol for diffuse. It was shown that after annealing at 663 K coercivity decrease about 30% and therefore substantial reduction in power loses was attained. Investigated amorphous alloy satisfied the criteria for signal processing devices that work in mean frequency domain.",
publisher = "Belgrade : ETRAN",
journal = "Science of Sintering",
title = "The effect of temperature and frequency on magnetic properties of the Fe81B13Si4C2 amorphous alloy",
pages = "175-182",
volume = "43",
number = "2",
doi = "10.2298/SOS1102175D",
url = "https://hdl.handle.net/21.15107/rcub_dais_16291"
}
Đukić, S., Maričić, V., Kalezić Glišović, A., Ribić Zelenović, L., Ranđić, S., Mitrović, N.,& Obradović, N.. (2011). The effect of temperature and frequency on magnetic properties of the Fe81B13Si4C2 amorphous alloy. in Science of Sintering
Belgrade : ETRAN., 43(2), 175-182.
https://doi.org/10.2298/SOS1102175D
https://hdl.handle.net/21.15107/rcub_dais_16291
Đukić S, Maričić V, Kalezić Glišović A, Ribić Zelenović L, Ranđić S, Mitrović N, Obradović N. The effect of temperature and frequency on magnetic properties of the Fe81B13Si4C2 amorphous alloy. in Science of Sintering. 2011;43(2):175-182.
doi:10.2298/SOS1102175D
https://hdl.handle.net/21.15107/rcub_dais_16291 .
Đukić, S., Maričić, V., Kalezić Glišović, Aleksandra, Ribić Zelenović, Lenka, Ranđić, Siniša, Mitrović, Nebojša, Obradović, Nina, "The effect of temperature and frequency on magnetic properties of the Fe81B13Si4C2 amorphous alloy" in Science of Sintering, 43, no. 2 (2011):175-182,
https://doi.org/10.2298/SOS1102175D .,
https://hdl.handle.net/21.15107/rcub_dais_16291 .
3
9
9

Correlation between isothermal expansion and functional properties change of the Fe81B13Si4C2 amorphous alloy

Kalezić Glišović, Aleksandra; Maričić, V. A.; Kosanović, Darko; Đukić, S.; Simeunović, R.

(Belgrade : International Institute for the Science of Sintering, 2009)

TY  - JOUR
AU  - Kalezić Glišović, Aleksandra
AU  - Maričić, V. A.
AU  - Kosanović, Darko
AU  - Đukić, S.
AU  - Simeunović, R.
PY  - 2009
UR  - https://dais.sanu.ac.rs/123456789/206
AB  - The structural changes effect on functional properties of ribbon shaped samples of the Fe81B13Si4C2 amorphous alloy during annealing process was investigated in this paper. Differential scanning calorimetry method has shown that this alloy crystallizes in one stage, in temperature range from room temperature up to 700°C. Structural relaxation process was investigated by sensitive dilatation method in nonisothermal and isothermal conditions. It has been shown that structural relaxation process occurs in two stages by measuring thermal expansion at constant temperatures of t1=420°C, t2 = 440°C and t3 = 460°C. The first stage is characterized by linear logarithmic dependence of thermal expansion upon time at constant temperature. The second stage of structural relaxation process is characterized by linear dependence of isothermal expansion upon the square root of process time. These results imply that the first stage of structural relaxation process is a rapid kinetic process, while the second stage of structural relaxation process is a slow diffusion process. The rate constants k11 = 2,27⋅10- 3 s-1, k12 = 2,79⋅10-3 s-1, k13 = 3,6⋅10-3 s-1, k21 = 0,67⋅10-4 s-1, k22 = 3,72⋅10-4 s-1, k23 = 21,53⋅10-4 s-1 and activation energies E1 = 48,64 kJ/mol and E2 = 366, 23 kJ/mol were determined for both stages of structural relaxation process. The distinct correlation between structural relaxation process and magnetic susceptibility relative change was determined by thermomagnetic measurements. It has been shown that magnetic susceptibility can be increased by up to 80%, by convenient annealings after structural relaxation process, at magnetic field intensity of 8 kA/m.
PB  - Belgrade : International Institute for the Science of Sintering
T2  - Science of Sintering
T1  - Correlation between isothermal expansion and functional properties change of the Fe81B13Si4C2 amorphous alloy
SP  - 283
EP  - 291
VL  - 41
IS  - 3
DO  - 10.2298/SOS0903283K
UR  - https://hdl.handle.net/21.15107/rcub_dais_206
ER  - 
@article{
author = "Kalezić Glišović, Aleksandra and Maričić, V. A. and Kosanović, Darko and Đukić, S. and Simeunović, R.",
year = "2009",
abstract = "The structural changes effect on functional properties of ribbon shaped samples of the Fe81B13Si4C2 amorphous alloy during annealing process was investigated in this paper. Differential scanning calorimetry method has shown that this alloy crystallizes in one stage, in temperature range from room temperature up to 700°C. Structural relaxation process was investigated by sensitive dilatation method in nonisothermal and isothermal conditions. It has been shown that structural relaxation process occurs in two stages by measuring thermal expansion at constant temperatures of t1=420°C, t2 = 440°C and t3 = 460°C. The first stage is characterized by linear logarithmic dependence of thermal expansion upon time at constant temperature. The second stage of structural relaxation process is characterized by linear dependence of isothermal expansion upon the square root of process time. These results imply that the first stage of structural relaxation process is a rapid kinetic process, while the second stage of structural relaxation process is a slow diffusion process. The rate constants k11 = 2,27⋅10- 3 s-1, k12 = 2,79⋅10-3 s-1, k13 = 3,6⋅10-3 s-1, k21 = 0,67⋅10-4 s-1, k22 = 3,72⋅10-4 s-1, k23 = 21,53⋅10-4 s-1 and activation energies E1 = 48,64 kJ/mol and E2 = 366, 23 kJ/mol were determined for both stages of structural relaxation process. The distinct correlation between structural relaxation process and magnetic susceptibility relative change was determined by thermomagnetic measurements. It has been shown that magnetic susceptibility can be increased by up to 80%, by convenient annealings after structural relaxation process, at magnetic field intensity of 8 kA/m.",
publisher = "Belgrade : International Institute for the Science of Sintering",
journal = "Science of Sintering",
title = "Correlation between isothermal expansion and functional properties change of the Fe81B13Si4C2 amorphous alloy",
pages = "283-291",
volume = "41",
number = "3",
doi = "10.2298/SOS0903283K",
url = "https://hdl.handle.net/21.15107/rcub_dais_206"
}
Kalezić Glišović, A., Maričić, V. A., Kosanović, D., Đukić, S.,& Simeunović, R.. (2009). Correlation between isothermal expansion and functional properties change of the Fe81B13Si4C2 amorphous alloy. in Science of Sintering
Belgrade : International Institute for the Science of Sintering., 41(3), 283-291.
https://doi.org/10.2298/SOS0903283K
https://hdl.handle.net/21.15107/rcub_dais_206
Kalezić Glišović A, Maričić VA, Kosanović D, Đukić S, Simeunović R. Correlation between isothermal expansion and functional properties change of the Fe81B13Si4C2 amorphous alloy. in Science of Sintering. 2009;41(3):283-291.
doi:10.2298/SOS0903283K
https://hdl.handle.net/21.15107/rcub_dais_206 .
Kalezić Glišović, Aleksandra, Maričić, V. A., Kosanović, Darko, Đukić, S., Simeunović, R., "Correlation between isothermal expansion and functional properties change of the Fe81B13Si4C2 amorphous alloy" in Science of Sintering, 41, no. 3 (2009):283-291,
https://doi.org/10.2298/SOS0903283K .,
https://hdl.handle.net/21.15107/rcub_dais_206 .
5
7
7