Correlation between isothermal expansion and functional properties change of the Fe81B13Si4C2 amorphous alloy
2009
Аутори
Kalezić Glišović, AleksandraMaričić, V. A.
Kosanović, Darko
Đukić, S.
Simeunović, R.
Остала ауторства
Ristić, Momčilo M.Чланак у часопису (Објављена верзија)
Метаподаци
Приказ свих података о документуАпстракт
The structural changes effect on functional properties of ribbon shaped samples of the Fe81B13Si4C2 amorphous alloy during annealing process was investigated in this paper. Differential scanning calorimetry method has shown that this alloy crystallizes in one stage, in temperature range from room temperature up to 700°C. Structural relaxation process was investigated by sensitive dilatation method in nonisothermal and isothermal conditions. It has been shown that structural relaxation process occurs in two stages by measuring thermal expansion at constant temperatures of t1=420°C, t2 = 440°C and t3 = 460°C. The first stage is characterized by linear logarithmic dependence of thermal expansion upon time at constant temperature. The second stage of structural relaxation process is characterized by linear dependence of isothermal expansion upon the square root of process time. These results imply that the first stage of structural relaxation process is a rapid kinetic process, while the s...econd stage of structural relaxation process is a slow diffusion process. The rate constants k11 = 2,27⋅10- 3 s-1, k12 = 2,79⋅10-3 s-1, k13 = 3,6⋅10-3 s-1, k21 = 0,67⋅10-4 s-1, k22 = 3,72⋅10-4 s-1, k23 = 21,53⋅10-4 s-1 and activation energies E1 = 48,64 kJ/mol and E2 = 366, 23 kJ/mol were determined for both stages of structural relaxation process. The distinct correlation between structural relaxation process and magnetic susceptibility relative change was determined by thermomagnetic measurements. It has been shown that magnetic susceptibility can be increased by up to 80%, by convenient annealings after structural relaxation process, at magnetic field intensity of 8 kA/m.
Кључне речи:
amorphous materials / structural relaxation / thermal expansion / magnetic susceptibilityИзвор:
Science of Sintering, 2009, 41, 3, 283-291Издавач:
- Belgrade : International Institute for the Science of Sintering
Финансирање / пројекти:
- Проучавање међузависности у тријади ''синтеза-структура-својства'' за функционалне материјала (RS-MESTD-MPN2006-2010-142011)
DOI: 10.2298/SOS0903283K
ISSN: 1820-7413; 0350-820X
WoS: 000275835500006
Scopus: 2-s2.0-76649102450
Институција/група
Институт техничких наука САНУ / Institute of Technical Sciences of SASATY - JOUR AU - Kalezić Glišović, Aleksandra AU - Maričić, V. A. AU - Kosanović, Darko AU - Đukić, S. AU - Simeunović, R. PY - 2009 UR - https://dais.sanu.ac.rs/123456789/206 AB - The structural changes effect on functional properties of ribbon shaped samples of the Fe81B13Si4C2 amorphous alloy during annealing process was investigated in this paper. Differential scanning calorimetry method has shown that this alloy crystallizes in one stage, in temperature range from room temperature up to 700°C. Structural relaxation process was investigated by sensitive dilatation method in nonisothermal and isothermal conditions. It has been shown that structural relaxation process occurs in two stages by measuring thermal expansion at constant temperatures of t1=420°C, t2 = 440°C and t3 = 460°C. The first stage is characterized by linear logarithmic dependence of thermal expansion upon time at constant temperature. The second stage of structural relaxation process is characterized by linear dependence of isothermal expansion upon the square root of process time. These results imply that the first stage of structural relaxation process is a rapid kinetic process, while the second stage of structural relaxation process is a slow diffusion process. The rate constants k11 = 2,27⋅10- 3 s-1, k12 = 2,79⋅10-3 s-1, k13 = 3,6⋅10-3 s-1, k21 = 0,67⋅10-4 s-1, k22 = 3,72⋅10-4 s-1, k23 = 21,53⋅10-4 s-1 and activation energies E1 = 48,64 kJ/mol and E2 = 366, 23 kJ/mol were determined for both stages of structural relaxation process. The distinct correlation between structural relaxation process and magnetic susceptibility relative change was determined by thermomagnetic measurements. It has been shown that magnetic susceptibility can be increased by up to 80%, by convenient annealings after structural relaxation process, at magnetic field intensity of 8 kA/m. PB - Belgrade : International Institute for the Science of Sintering T2 - Science of Sintering T1 - Correlation between isothermal expansion and functional properties change of the Fe81B13Si4C2 amorphous alloy SP - 283 EP - 291 VL - 41 IS - 3 DO - 10.2298/SOS0903283K UR - https://hdl.handle.net/21.15107/rcub_dais_206 ER -
@article{ author = "Kalezić Glišović, Aleksandra and Maričić, V. A. and Kosanović, Darko and Đukić, S. and Simeunović, R.", year = "2009", abstract = "The structural changes effect on functional properties of ribbon shaped samples of the Fe81B13Si4C2 amorphous alloy during annealing process was investigated in this paper. Differential scanning calorimetry method has shown that this alloy crystallizes in one stage, in temperature range from room temperature up to 700°C. Structural relaxation process was investigated by sensitive dilatation method in nonisothermal and isothermal conditions. It has been shown that structural relaxation process occurs in two stages by measuring thermal expansion at constant temperatures of t1=420°C, t2 = 440°C and t3 = 460°C. The first stage is characterized by linear logarithmic dependence of thermal expansion upon time at constant temperature. The second stage of structural relaxation process is characterized by linear dependence of isothermal expansion upon the square root of process time. These results imply that the first stage of structural relaxation process is a rapid kinetic process, while the second stage of structural relaxation process is a slow diffusion process. The rate constants k11 = 2,27⋅10- 3 s-1, k12 = 2,79⋅10-3 s-1, k13 = 3,6⋅10-3 s-1, k21 = 0,67⋅10-4 s-1, k22 = 3,72⋅10-4 s-1, k23 = 21,53⋅10-4 s-1 and activation energies E1 = 48,64 kJ/mol and E2 = 366, 23 kJ/mol were determined for both stages of structural relaxation process. The distinct correlation between structural relaxation process and magnetic susceptibility relative change was determined by thermomagnetic measurements. It has been shown that magnetic susceptibility can be increased by up to 80%, by convenient annealings after structural relaxation process, at magnetic field intensity of 8 kA/m.", publisher = "Belgrade : International Institute for the Science of Sintering", journal = "Science of Sintering", title = "Correlation between isothermal expansion and functional properties change of the Fe81B13Si4C2 amorphous alloy", pages = "283-291", volume = "41", number = "3", doi = "10.2298/SOS0903283K", url = "https://hdl.handle.net/21.15107/rcub_dais_206" }
Kalezić Glišović, A., Maričić, V. A., Kosanović, D., Đukić, S.,& Simeunović, R.. (2009). Correlation between isothermal expansion and functional properties change of the Fe81B13Si4C2 amorphous alloy. in Science of Sintering Belgrade : International Institute for the Science of Sintering., 41(3), 283-291. https://doi.org/10.2298/SOS0903283K https://hdl.handle.net/21.15107/rcub_dais_206
Kalezić Glišović A, Maričić VA, Kosanović D, Đukić S, Simeunović R. Correlation between isothermal expansion and functional properties change of the Fe81B13Si4C2 amorphous alloy. in Science of Sintering. 2009;41(3):283-291. doi:10.2298/SOS0903283K https://hdl.handle.net/21.15107/rcub_dais_206 .
Kalezić Glišović, Aleksandra, Maričić, V. A., Kosanović, Darko, Đukić, S., Simeunović, R., "Correlation between isothermal expansion and functional properties change of the Fe81B13Si4C2 amorphous alloy" in Science of Sintering, 41, no. 3 (2009):283-291, https://doi.org/10.2298/SOS0903283K ., https://hdl.handle.net/21.15107/rcub_dais_206 .