Претраживање
Приказ резултата 1-2 од 2
Structural characterization of mechanically activated MgO-TiO2 system
(Belgrade : Materials Research Society of Serbia, 2011)
Mixtures of MgO-TiO2 powders were mechanically activated in a planetary ball mill for time interval from 0 to 120 minutes. On thus obtained powders, structural investigations have been performed. N2 adsorption method was ...
Sintering of mechanically activated MgO-TiO2 system
(Belgrade : Institute of Technical Sciences of SASA, 2011)
Mixtures of MgO-TiO2 powders were mechanically activated in planetary ball mill for time interval from 0 to 120 minutes. The influence of mechanical activation on phase composition and crystal structure was analyzed by ...