Spark plasma sintering of magnesium titanate ceramics
(Ceramics International, 2024)
Magnesium titanate ceramics were prepared by reactive spark plasma sintering (SPS) at 1200 °C for 5 min. Prior to sintering, MgO and TiO2 powders were mixed by high energy ball milling (HEBM) for 15, 30, or 60 min. The ...