Structural analysis of Zn2TiO4 doped with MgO
(Springer, 2009)
The starting mixtures of ZnO, TiO2, and MgO (0, 1.25, and 2.5 wt.%) powders are mechanically activated in a high-energy planetary mill for 15 min and then sintered between 800 and 1100°C for 2 h. The influence of MgO ...
Densification rate and phase structure changes during sintering of zinc titanate ceramics
(Elsevier, 2009)
Densification rate and phase structure changes during sintering of nanosized ZnTiO3 were studied. Sintering was performed in a dilatometer in two regimes: the first to 900 °C (heating rates 5, 10 and 15 °C/min) and the ...
Structural and Electrical Properties of Sintered Zinc-titanate Ceramics
(2005)
Poster presented at the ELECTROCERAMICS X, June 18-22, 2006, Toledo, Spain
The Influence of Milling Conditions on Mechanochemical Synthesis and Sintering of Zinc Titanate
(Kyiv : G. V. Kurdyumov Institute for Metal Physics of the National Academy of Sciences of Ukraine, 2006)
The aim of this work was an investigation of experimental conditions for mechanochemical synthesis and sintering of spinel zinc titanate (Zn2TiO4). Starting powder mixtures of zinc oxide and titan dioxide in the molar ...
Enhancing Synthesis and Sintering of Zinc Titanate Using Mechanical Activation
(Progress in Advanced Materials and Processes, 2004)
Mechanical activation and sintering are used for obtaining zinc titanate, Zn2TiO4. Starting powder mixtures of ZnO and TiO2, in the molar ratio that is in accordance with the stoichiometry ofzinc titanate Zn2TiO4, were ...