Претраживање
Приказ резултата 1-5 од 5
Structural analysis of Zn2TiO4 doped with MgO
(Springer, 2009)
The starting mixtures of ZnO, TiO2, and MgO (0, 1.25, and 2.5 wt.%) powders are mechanically activated in a high-energy planetary mill for 15 min and then sintered between 800 and 1100°C for 2 h. The influence of MgO ...
Far infrared reflectance of sintered Zn2TiO4
(Springer Science+Business Media, 2008)
Zinc-titanate ceramics were obtained by initial mechanical activation in a high-energy planetary mill for 15 min followed by sintering at temperatures 900-1100°C for 2 h. Room temperature far infrared reflectivity spectra ...
Sintering of mechanically activated Zno-TiO 2 powders
(Springer, 2008)
Zinc oxide and titanium dioxide powders mixed in an equimolar ratio are mechanically activated in a planetary ball mill and sintered under nonisothermal and isothermal conditions. Nonisothermal sintering is studied using ...
Enhancing Synthesis and Sintering of Zinc Titanate Using Mechanical Activation
(Progress in Advanced Materials and Processes, 2004)
Mechanical activation and sintering are used for obtaining zinc titanate, Zn2TiO4. Starting powder mixtures of ZnO and TiO2, in the molar ratio that is in accordance with the stoichiometry ofzinc titanate Zn2TiO4, were ...
The influence of mechanical activation on the stoichiometry and defect structure of a sintered ZnO-Cr2O3 system / The influence of mechanical activation on the stoichiometry and defect structure of a sintered ZnO-Cr2O3 system
(Zurich : Trans Tech Publications, 2004)
Mixtures of starting ZnO and Cr2O3 powders in equimolar quantities were mechanically activated by grinding using a high energy vibro-mill for 0, 40 and 80 minutes. Qualitative X-ray diffraction analysis made after sintering ...