The influence of mechanical activation on the electrical properties of Ba0.77Sr0.23TiO3 ceramics
(Belgrade : Serbian Ceramic Society, 2013)
Ferroelectric ceramic barium strontium titanate (Ba0.77Sr0.23TiO3), BST, was prepared by solid-state reactions using starting powders of barium carbonate (BaCO3), strontium carbonate (SrCO3) and titanium dioxide (TiO2-anatase). ...
Microstructural and electrical properties of cordierite-based ceramics obtained after two-step sintering technique
(Science of Sintering, 2016)
Cordierite-based ceramic materials are attracting much interest for their various applications in industry, for manufacturing multilayer circuit boards, catalytic converters, filters, thermal insulation, kiln furniture, ...
The influence of mechanical activation on the electrical properties of Ba0.77Sr0.23TiO3
(2013)
Poster presented at the conference Advanced Ceramics and Application II – Serbian Ceramic Society, Belgrade, September 30 – October 1, 2013
Influence of Mechanical Activation on Electrical Properties of Ceramic Materials in VHF Band
(Belgrade : ETRANBelgrade : Academic Mind, 2019)
Mechanical activation is commonly used as a pre-sintering process in order to enhance the reactivity of materials, reduce the particle size, increase diffusion rates, accelerate the reaction, and lower the sintering ...
Influence of prolonged sintering time on density and electrical properties of isothermally sintered cordierite-based ceramics
(Belgrade : International Institute for the Science of Sintering, 2013)
Mechanical activation is a commonly used and relatively fast and inexpensive procedure for sample preparation before the sintering process. Cordierite, a stoichiometric mixture of three different oxides (2MgO⋅2Al2O3⋅5SiO2) ...
The influence of compaction pressure on the density and electrical properties of cordierite-based ceramics
(Belgrade : International Institute for the Science of Sintering, 2015)
Due to its characteristics, cordierite, 2MgO·2Al2O3·5SiO2, is a high-temperature ceramic material of a great scientific interest. Mechanical activation of the starting mixtures containing 5.00 mass% TiO2 was performed in ...