Nanomechanical properties of PVDF–ZnO polymer nanocomposite
(Elsevier BV, 2023)
Poly(vinylidenefluoride)–ZnO (PVDF–ZnO) nanocomposites with mechanically activated ZnO nanoparticle fillers were investigated using thermal and mechanical analysis and AFM and PFM. Differential scanning calorimetry (DSC) ...
Nanomechanical properties of PVDF–ZnO polymer nanocomposite
(Elsevier BV, 2023)
Poly(vinylidenefluoride)–ZnO (PVDF–ZnO) nanocomposites with mechanically activated ZnO nanoparticle fillers were investigated using thermal and mechanical analysis and AFM and PFM. Differential scanning calorimetry (DSC) ...